Different materials have different saturation levels. For example, high permeability iron alloys used in transformers reach magnetic saturation at 1.6–2.2teslas (T), whereas ferrites saturate at 0.2–0.5T. Some amorphous alloys saturate at 1.2–1.3T. Mu-metal saturates at around 0.8T.